0.8mm E71t-1 Welding Wire, Building Materials, Welding Materials Factory Direct Sales

Product Name: 0.8mm E71t-1 Welding Wire SEO Description: Get high-quality 0.8mm E71t-1 welding wire directly from the factory. We are a leading manufacturer of building and welding materials.
Request a Quote

PRODUCTS DETAILS

Basic Info.

Model NO.
E71T-1
Spool/Reel
D100, D200, D270, D300, K300
Transport Packaging
3tons/Pallet
Color
Copper
Splash
Low
Strength
High
Transport Package
Pallet
Specification
0.8mm 1.0mm 1.2mm
Trademark
WP
Origin
Shandong
HS Code
72292000
Production Capacity
30000tons/Year

Product Description

 

 

0.8mm E71t-1 Welding Wire, Building Materials, Welding Materials Factory Direct Sales 0.8mm E71t-1 Welding Wire, Building Materials, Welding Materials Factory Direct Sales 0.8mm E71t-1 Welding Wire, Building Materials, Welding Materials Factory Direct Sales
Model NO. AWS ER70S-6 Spool/Reel D100, D200, D270, D300, K300
Shielded Gas CO2 Specification 3tons/Pallet
Transport Package OEM Origin CHINA
HS Code 72292000 Production Capacity 2000tons Per Months
Product Name ER70S-6 CO2 gas shielded welding wires
Keywords welding wire
Material Stainless steel
Color copper
Grade ER70S-6
Size Available Diameters:0.8mm / 0.9mm/ 1.0mm / 1.2mm / 1.6mm / 2.0mm / 2.4mm etc..
Weight 1KG/2KG/6KG /7KG/10KG /15KG/20KG per spool, or by bundle
Explanation It has strong resistance to surface oxidation and oil stains on the base material,and low sensitivity to pores.
Used bridges, buildings, shipbuilding,machinery, automobiles, pressure vessels, as well as for welding plates and pipes
0.8mm E71t-1 Welding Wire, Building Materials, Welding Materials Factory Direct Sales 0.8mm E71t-1 Welding Wire, Building Materials, Welding Materials Factory Direct Sales 0.8mm E71t-1 Welding Wire, Building Materials, Welding Materials Factory Direct Sales
0.8mm E71t-1 Welding Wire, Building Materials, Welding Materials Factory Direct Sales

Chemical omposition of welding wire:(%)

  C Mn Si S p Cu
standard value
 
0.06-0.15 1.40-1.85 0.80-1.15 ≤0.035 ≤0.025 ≤0.50
sample value
 
0.080  1.510  0.920  0.020  0.016  0.200 
Chemical omposition of deposited matal:(%)
C Mn Si S P Cu
0.070  1.500  0.760  0.014  0.015  0.150 
Mechanical properties of deposited metal:(%)
  Tensile strength
δb(MPa)
Yield Point
δ0.2(Mpa)
Elongation
δ5(%)
AKV Impact Value
(J)(-30ºC)
Shielding gas
Standard value

 
≥500 ≥420 ≥22 27 CO2
Typical value 558 472 27 98 CO2
Property:Our company's welding wire is produced by high technology of copper coating, which surface is smooth and shiny, the copper layer is uniform and tight. We adopt the alignment technology and the CO2 gas shielded welding wire has excellent welding technological properties: stable electric arc, low splashing, beautiful welding seams, high deposition efficiency, etc.This series of welding wire is suitable for all positions and semi-auto and automatic gas shielded welding.
Application:CO2 gas shielded welding wire is mainly used in the welding of low carbon steel and 500Mpa grade alloy steel structure parts. Also used in all kinds of 500 Mpa grade steel board and pipe welding work. It is widely used in the area of vehicles, bridges, construction machinery, pressure vessel, engineering structures and container buildings etc.
Diameter of wire& reference current(DC+)
Diameter of wire (mm) Φ0.8 Φ1.0 Φ1.2 Φ1.6
current (A) 40-140 70-250 80-350 170-550
Arc voltage(V) 16-21 17-27 18-30 23
 
0.8mm E71t-1 Welding Wire, Building Materials, Welding Materials Factory Direct Sales 0.8mm E71t-1 Welding Wire, Building Materials, Welding Materials Factory Direct Sales 0.8mm E71t-1 Welding Wire, Building Materials, Welding Materials Factory Direct Sales 0.8mm E71t-1 Welding Wire, Building Materials, Welding Materials Factory Direct Sales





















 