Stainless Steel Weldig Wire
Specifications:
AWS A5.9
AWS ER308/ ER308L
ASME SFA 5.9
UNS S30880/ S30883
Description:
ER308L contains low carbon material that reduces the possibility of intergranular carbide precipitation. This increases the resistance to intergranular corrosion without the use of stabilizers such as niobium or titanium. ER308L wire is designed for welding and overlay of base metals similar in composition, such as 304L. 308L is well suited for applications in the chemical and petrochemical industries, distilleries, dairy, and restaurant equipment; and in applications where a good atmospheric corrosion resistance is needed.
Available sizes and diameters and packing details:
MIG diameter | 0.8mm 0.9mm 1.0mm 1.2mm 1.6mm |
TIG diameter | 1.6mm 2.0mm 2.4mm 3.0mm 3.2mm 4.0mm |
Raw material | stainless steel alloy |
MIG Packing | 1kg/spool, 5kg/spool, 7kg/spool/15kg/spool |
TIG packing | 5kg/plastic tube |
Chemical Compositions of Stainless Steel Welding Wire:
C | Si | Mn | P | S | Cr | Ni | Mo | Cu | |
304 | 0.08 | 0.30-1.00 | 2.00 | 0.045 | 0.030 | 18.00-20.00 | 8.00-11.00 | 0.18 | 0.003 |
304L | 0.03 | 0.30-1.00 | 2.00 | 0.045 | 0.030 | 18.00-20.00 | 8.00-12.00 | ||
ER307 | 0.04-0.14 | 0.30-0.65 | 4.30-4.75 | 0.030 | 0.030 | 19.50-22.00 | 8.00-10.70 | 0.5-1.5 | 0.75 |
ER308 | 0.08 | 0.30-0.65 | 4.30-4.75 | 0.030 | 0.030 | 19.50-22.00 | 9.00-11.00 | 0.75 | 0.75 |
ER308L | 0.03 | 0.30-0.65 | 1.50-2.30 | 0.03 | 0.02 | 19.5-21.5 | 9.00-11.00 | 0.75 | 0.75 |
ER308LSi | 0.03 | 0.65-1.00 | 1.60-2.40 | 0.03 | 0.02 | 19.5-21.5 | 9.0-11.0 | 0.75 | 0.75 |
ER309 | 0.12 | 0.30-0.65 | 1.00-2.50 | 0.03 | 0.03 | 24.0-25.0 | 12.0-14.0 | 0.75 | 0.75 |
ER309L | 0.03 | 0.3-0.65 | 1.5-2.3 | 0.03 | 0.02 | 23.0-25.0 | 12.0-14.0 | 0.75 | 0.75 |
ER309LSi | 0.03 | 0.65-1.0 | 1.6-2.4 | 0.03 | 0.02 | 23.0-25.0 | 12.0-14.0 | 0.75 | 0.75 |
ER316 | 0.08 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.03 | 18.00-12.00 | 11.0-14.0 | 2.0-3.0 | 0.75 |
ER316L | 0.03 | 0.3-0.65 | 1.5-2.3 | 0.03 | 0.02 | 18.0-20.0 | 11.0-13.0 | 2.05-2.55 | 0.75 |
ER316LSi | 0.03 | 0.65-1.0 | 1.6-2.4 | 0.03 | 0.02 | 18.0-20.0 | 11.0-13.0 | 2.05-2.55 | 0.75 |
ER310 | 0.08-0.15 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.03 | 25.0-28.0 | 20.0-22.5 | 0.75 | 0.75 |
ER347 | 0.08 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.03 | 19.0-21.5 | 9.0-11.0 | 0.75 | 0.75 |
ER317 | 0.08 | 0.3-0.65 | 1.0-2.5 | 0.03 | 0.01 | 18.5-20.5 | 13.0-15.0 | 3.0-4.0 | 0.75 |
ER321 | 0.08 | 0.3-0.65 | 1.5-2.5 | 0.03 | 0.01 | 18.5-20.5 | 9.0-10.5 | 0.75 | 0.75 |
Mechanical Properties of Welding Wire:
Tensile strength Rm(Mpa) | Yield strength Rel or Rp0.2(Mpa) | Elongation(%) | Tensile strength Rm(Mpa) | Yield strength Rel or Rp0.2(Mpa) | Elongation(%) | ||
304 | 550 | -- | 25 | ER309LSi | 510 | 320 | 25 |
304L | 510 | -- | 25 | ER316 | 510 | 320 | 25 |
ER307 | 590 | 350 | 25 | ER316L | 510 | 320 | 25 |
ER308 | 550 | 350 | 25 | ER316LSi | 510 | 320 | 20 |
ER308L | 510 | 320 | 25 | ER310 | 550 | 350 | 25 |
ER308LSi | 510 | 320 | 25 | ER347 | 550 | 350 | 25 |
ER309 | 550 | 350 | 25 | ER317 | 550 | 350 | 25 |
ER309L | 510 | 320 | 25 | ER321 | 550 | 350 | 25 |
Chemical compostiton of deposited metal (shield gas:CO2)
C | Mn | Si | P | S | Ni | Cr |
0.03 | 1.42 | 0.42 | 0.027 | 0.004 | 9.81 | 19.83 |
Mechanical properties of deposited metal (shield gas:CO2
Yield Strength | Elongation | Impact Value |
Mpa(σb) | %(δ5) | 0ºC(J) |
570 | 43 | 41 |
Sizes available and recommended currents(DC-EP)
Diameter(mm) | 0.9 | 1.2 | 1.6 | |
Current(A) | F,HF | 130-180 | 180-220 | 250-290 |
V-up OH | 100-140 | 120-160 | 220-270 |